IMPROVING METHOD FOR HIGH FREQUENCY MAGNETIC PROPE
合集下载
- 1、下载文档前请自行甄别文档内容的完整性,平台不提供额外的编辑、内容补充、找答案等附加服务。
- 2、"仅部分预览"的文档,不可在线预览部分如存在完整性等问题,可反馈申请退款(可完整预览的文档不适用该条件!)。
- 3、如文档侵犯您的权益,请联系客服反馈,我们会尽快为您处理(人工客服工作时间:9:00-18:30)。
申请人:MITSUBISHI METAL CORP
更多信息请下载全文后查看
申请号:J P 1024 7586 申请日:19860502 公开号:J P S622594 08A 公开日:19871111
摘要:PURPOSE:To improve the high frequency magnetic property of a soft magnetic Fe-Si alloy member by specifying the thickness of a surface layer to be hardened or deformed and the ratio of the sectional area thereof. CONSTITUTION:A surface layer having 50-1000mum of thickness of a magnetically soft Fe-Si alloy member along the flow of a magnetic flux passing the center of the member of a surface layer of the member disposed in an alternating magnetic field and a magnetic field of predetermined direction flows is so hardened or deformed that the ratio of the sectional area occupying the surface layer in the thicknesswise section of the surface layer is 2-40% of the area of the entire section. Thus, since the high frequency magnetic property of the member is remarkably improved. The surface layer except thቤተ መጻሕፍቲ ባይዱ specific surface layer region and the interior of the member are not hardened nor deformed together with the above property, the alloy itself can hold the excellent original magnetic property as it is.
专利内容由知识产权出版社提供
专利名称:IMPROVING METHOD FOR HIGH FREQUENCY MAGNETIC PROPERTY OF MAGNETICALLY SOFT FE-SI ALLOY MEMBER
发明人:WAKITA SABURO,YAMAGUCHI SEIJI,ANZAI KO
更多信息请下载全文后查看
申请号:J P 1024 7586 申请日:19860502 公开号:J P S622594 08A 公开日:19871111
摘要:PURPOSE:To improve the high frequency magnetic property of a soft magnetic Fe-Si alloy member by specifying the thickness of a surface layer to be hardened or deformed and the ratio of the sectional area thereof. CONSTITUTION:A surface layer having 50-1000mum of thickness of a magnetically soft Fe-Si alloy member along the flow of a magnetic flux passing the center of the member of a surface layer of the member disposed in an alternating magnetic field and a magnetic field of predetermined direction flows is so hardened or deformed that the ratio of the sectional area occupying the surface layer in the thicknesswise section of the surface layer is 2-40% of the area of the entire section. Thus, since the high frequency magnetic property of the member is remarkably improved. The surface layer except thቤተ መጻሕፍቲ ባይዱ specific surface layer region and the interior of the member are not hardened nor deformed together with the above property, the alloy itself can hold the excellent original magnetic property as it is.
专利内容由知识产权出版社提供
专利名称:IMPROVING METHOD FOR HIGH FREQUENCY MAGNETIC PROPERTY OF MAGNETICALLY SOFT FE-SI ALLOY MEMBER
发明人:WAKITA SABURO,YAMAGUCHI SEIJI,ANZAI KO